Surface Resistance Test Method:ASTM D257
Tear Strength:100 N/mm
Material:Polyethylene
Elongation At Break Test Method:ASTM D882
Surface Finish:Smooth/Matte
Closure Type:Self-seal
Surface Resistance Test Method:ASTM D257
Puncture Resistance:50 N
Closure Type:Self-seal
Certifications:RoHS, REACH, And ISO 9001:2015
Tensile Strength Test Method:ASTM D882
Material:Polyethylene
Surface Resistance Test Method:ASTM D257
Surface Resistance:10^6 - 10^11 ohms
Size:Customizable
Static Decay Time:Less Than 2 Seconds
Closure Type:Self-seal
Air Bubbles Diameter:10,25or30mm
Certifications:RoHS, REACH, and ISO 9001:2015
Seal Type:Heat Seal
Puncture Resistance:More than 100 lbs
Minimum Order Quantity:100pcs
Цена:Discussable
Packaging Details:Box
Метериал:PE
Стандартный:Соответствие требованиям ESD Mil-B-81705B
Сопротивление поверхности:< 1012 Омм/кв. м